“Without a skilled driver, a performance Race Car is only as good as the sum of its component parts.”
In 2013 Artisan refined and perfected the application of black zinc electroplating for corrosion resistance up to 270 hours red corrosion in Neutral Salt Spray.
Using this same surface treatment as supplied to Toyota Motor Corporation and various other Manufacturing companies in Canada, Artisan helps Western Race team keep their Race Car corrosion free when they compete with 100 or so colleges and universities in Formula Racing.
In keeping with Artisan’s environmentally friendly approach to manufacturing, this process uses trivalent chromates and is applied at the minimum thickness to reduce waste while still maintain performance.